Monday, September 16, 2019

Re: [MW:30063] Aluminium welding failure from parent metal

Thanks for you reply. 
Kindly check the attached photos.

On Sun, 15 Sep 2019, 20:44 ViNo Varughese <vinopvarghese@gmail.com wrote:
Dear Kadir,

Can you please provide more information on the methodology tensile test was performed? Also refer to attach guideline which might be useful.

Thanks and Regards
Vino 
Qatar


On Sun, Sep 15, 2019, 16:01 <kadirgodil@gmail.com> wrote:
Dear experts,
EN AW 5754 H22 welded with ER5356, RT clear but gets failed in tensile.
What can be the reason please guide..
The artilce wleded is a 3 mm thick plate to plate butt joint.
Required YS 0.2 - 130 MPa
I am getting only 103 and 99 MPa.

Required UTS - 220-270 MPa
I am getting - 213 & 205 Mpa

Regards
Kadir godil

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/095b8b80-596a-4a0c-9cce-f2da1cbb7972%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM7oz7AFhFXYiO4Cx%3DTaVt0PU-gVMZ9RC_hqy9hXpeRDvsOgKQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKaLp%2BXLyqPOSaoObWcoz%2B3y9wsPhQkdDZOx%2BNo45Duo1-ZXKw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...