Wednesday, September 18, 2019

Re: [MW:30072] Re: WPS

Thanks Muneeb for such detailed explanation.
But in this case if the design or ambient temperature doesn't demand for any impact test than this supplementary essential variable shall not be applicable.
and hence the shown WPS can be used for weld between A106 and 105.
Please correct me if I am wrong.

thanks
Atul Khatri

On Tue, Sep 17, 2019 at 5:06 PM sellu....@gmai.com <selwinjebadass@gmail.com> wrote:
Hi,

i agree with muneeb's comment.

thanks.

On Friday, 23 August 2019 09:48:59 UTC+5:30, tusc...@gmail.com wrote:
dear all,

can I use the attached WPS for A106 pipe and A105 pipe fittings?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1bdef9de-63fd-45fc-9c34-4be0eb3bf7c9%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACKOSeCWrOWftyAE0JHmGar-BhsAGevG5cXHBXeTs9cffM1MBw%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...