Re: [MW:30055] Effect of Normalizing

Higher fibre elongations i guess.

Dinesh

On Sat, Sep 14, 2019, 16:48 Jayesh Parekh <jayeshparekh34@gmail.com> wrote:
 Normalizing heat treatment performed during dished end forming. As after Normalizing UTS and yield strength decreased. But due to which reason it is decreased ? what is process occured during normalizing that reduce uts and yield steength ? What metallurgy process occured during normalizing ? if any research paper is available please share. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/279983bf-c9fc-4695-8b35-f7502e4e387f%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAELgRrUeeZBWQxN8WNbfwRyY7O9e25GXRMM20wsAM%2B7XRy%2Bo0w%40mail.gmail.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...