Re: [MW:30019] SAW Hardfacing maximum thickness

Connect the Electrode in Negative terminal, u will get higher thickness. 

On Tue, 3 Sep 2019 9:26 am Ramin Kondori, <raminkondori@gmail.com> wrote:
Dear WeldBro,

Generally speaking, by using larger-diameter wires, increasing the overlap (much above normal 50%), lowering the travel speed, having a higher voltage and so forth, you can achieve layers with higher thickness. Of course, it all depends on the qualification test results which will eventually put a limit on it.

Regards   
Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Mon, Sep 2, 2019 at 7:35 PM Ashish Walia <itsashishwalia@gmail.com> wrote:
thanks for reply dinesh but i have heard of some ways by which even 12mm is achieved and i am curious to find out how is that possible i have myself reached upto 6mm

On Mon, Sep 2, 2019 at 4:26 PM Dinesh Somwanshi <som.din@gmail.com> wrote:

Generally its coming 3-4 mm.

On Sep 1, 2019 10:14 AM, "Weldbro" <itsashishwalia@gmail.com> wrote:
Can anyone suggest what is the maximum single layer thickness that can be achieved in SAW hardfacing. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/39f9b768-7fa6-47d9-a09c-4aaf59a22e19%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/XQfxQe8wT9E/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAELgRrVsVVeqsEnpyu9bRz-S4-%3DLsTjPKqJJ%2BpPQ6FrYsvZd-w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKas%2ByUwqHF5q%3DJLU4dOaYDVAm6LLtr-Bfb8s6eq2Q%2Bwrs3HNA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEagfUiiMZ%3DXtv8BoWiwHQKidO1w7g9LGzLu_SAU9y1hS1fy9w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePxGhyRrM3xJn6R_UokervN51-UPzSx-8jwiS2v7AUphQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...