[MW:30061] Re: SMAW +SAW

On Thursday, 5 September 2019 13:28:31 UTC+5:30, Dharma dattu wrote:
> Dear all,
> Need to establish a WPS For a project with PWHT root(full penetration by SMAW)and Subsequent layers by (SAW).
>
> My doubt is I have two seperate WPS for each procedure with PWHT separately.
>
> Can I submit both WPS to client and use them as one procedure on job
> 1. Root- full penetration joint - SMAW
> 2. SUB sequent layers - SAW
>
> NO Backgouging will be done.
> Root and finish to be UT 100%.
>
> REGARDS,
>
> DATTU.

Can I submit two WPS and do weld on a single job with both ( root&hot pass by SMAW and Subsequent layers by SAW)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5d30a79d-ee2a-45e8-94d7-0d7fb34acbba%40googlegroups.com.