Any body can clarify about  pre heating of ss  pipe joints  in -25°c climet  site work... need pre heating  or no... waiting for your valuable replay

On Fri, 13 Sep 2019, 5:39 pm Bien_ND / weldinginspections.net, <bck055@gmail.com> wrote:
Hello,

get free WPS and PQR format at

1- WPS for SMAW: https://lnkd.in/fevanEM 2- WPS for GTAW: https://lnkd.in/fzYnQKP 3- WPS for GTAW + FCAW: https://lnkd.in/fxMryha 4- WPS for GTAW + SMAW: https://lnkd.in/fQVJFN7 5- WPS for GTAW + SAW: https://lnkd.in/fjW6gvq 6- WPS for GTAW + GMAW: https://lnkd.in/fJ_mzK4



On Wednesday, September 11, 2019 at 3:51:59 PM UTC+7, Dharma dattu wrote:
Hello All,

we need to establish a wps with SMAW + SAW process, can you share the format.
my doubt is will it be called as welder qualification  or (welding operator qualification).

Regards,
DD

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3dc0931b-1f29-45e7-a4d6-66cc18f639d1%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD40ww_JX%3Dwcry0zzxC%2BoZ%2BsqdDVU5Ub%3D6f6F%2BeCJZ9ckQvA0g%40mail.gmail.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...