Dear Experts,
I would like to get your advice and opinion  about the welding og above subject.
We have to weld  1000 shear anchors on stainless steel 10 mm thick 
Following are the quality of the plate and anchor.
Plate      SA 240 Type 304
Shear Anchor    16x150mm S235J2+ C470
I would like to know whether we use  shear anchor welding machine to do the welding. These are the two different materials and chemical compositions are different we have to use  SS 309l welding rods and do the manual welding using SMAW or FCAW welding process.
Please give your valuable opinion.
Thanks in advance.
Cyriac Dominic

Virus-free. www.avast.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFMi6Sgw%2Btt7q6E169bTs8L%2BteXD6YZ3yFCkLfka_t-0rMZgJg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...