You should develope a new WPS compliant with Client's spec. and within the qualified range.
On Monday, September 9, 2019 at 4:31:02 PM UTC+7, Nhật Hoàng Bk wrote:
-- A qualified PQR may have one or two joint design combination at specific position.
So, there are no more type of groove design / joint details in the PQR.
On Monday, September 9, 2019 at 4:31:02 PM UTC+7, Nhật Hoàng Bk wrote:
Thank you very much.I don't know why summary PQR of my company or summary PQR of other company has all joint design (single V, single B, double V, double B). If 1 PQR with 1 joint design can qualify for other joint design, why they must cost money for them.(sorry, my english is not good)Thank ExpertsRegardsNguyễn Nhật HoàngVào Th 2, 9 thg 9, 2019 vào lúc 10:54 Bien_ND / weldinginspections.net <bck...@gmail.com> đã viết:On Thursday, September 5, 2019 at 10:15:44 AM UTC+7, Nhật Hoàng Bk wrote:
> Dear Experts,
>
>
> Could you please advise me for a question:
> I have a PQR qualifies single V, can I write WPS for single V, doubleV, single Bevel, double Bevel.
>
>
> Thank Experts
Reduce angle bevel are not allowed.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com .
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ .1deb3f5c-b994-4037-b596- fcb72c792fc0%40googlegroups. com
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c1e3c2a0-1b49-4597-8a88-07cd9537b6a0%40googlegroups.com.
Comments