Monday, September 9, 2019

Re: [MW:30044] Weep hole

Hi raghul,
Weep hole in dummy pipe is to vent out the heat and gases during welding.
you can have the weep hole in base plate as well.

On Mon, Sep 9, 2019 at 3:57 PM Raghul <raghul351991@gmail.com> wrote:
If weep hole is not provided in dummy pipe before welding
What will happen???

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACKOSeByZzwKAyRTdkr5Tj64PD3Lm0LJ7Ri6C96r%2BjOMyrAhdQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...