Yes , I don't see any issue.

On Thu, 5 Sep 2019 at 13:28, Dharma dattu <dharmadattu@gmail.com> wrote:
Dear all,
Need to establish a WPS For a project with PWHT root(full penetration by SMAW)and Subsequent layers by (SAW).

My doubt is I have two seperate WPS for each procedure with PWHT separately.

Can I submit both WPS to client and use them as one procedure on job
1. Root- full penetration joint - SMAW
2. SUB sequent layers - SAW

NO Backgouging will be done.
 Root and finish to be UT 100%.

REGARDS,

DATTU.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1fe7d9fd-d244-4aea-ae2d-8bcda3ae1316%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29OjDai6rUY4EVANrg3ujcsX7%3D-9iCjsu31%3DKSAf60%2B7BqQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...