Skip to main content

Re: [MW:29761] Re: Welding 4130 alloy

Dear Bien,
It's for structural welding application.
Thanks and Regards
Kiran 

On Wed, Jun 26, 2019 at 2:44 PM Bien_ND <bck055@gmail.com> wrote:
Hello,

In build up or hardbanding application?
E11018-M

Bien ND
QA/QC Engineer
weldinginspections.net

On Wednesday, June 26, 2019 at 12:47:09 PM UTC+7, ANANT wrote:
Dear,

Please can you tell me the process to do a welding on alloy 4130 material.   It is needed hardness values also. Approx 25 30 hrc. 

Which electrode are preferable...


On Tue, Jun 25, 2019, 16:57 Vinay Thattey <vinay....@gmail.com> wrote:
 I suggest you to Qualify in 3G . The 3G welding certification qualifies a welder to weld flat, horizontal, and vertical or 1G, 2G, and 3G positions, also includes the 1F, 2F, and 3F positions without having to take the 1G and 2G certification. This one test qualifies you for three positions.

On Thu, 20 Jun 2019 at 17:52, K K <kara...@gmail.com> wrote:
Dear Experts,

Please clarify me regarding below mentioned doubts.
As per AWS D1.1

1)      As per PQR thickness qualified with 25mm(Test coupon )


But In WPS thickness mentioned 28MM ( 3.2mm to unlimited )

 

As per AWS D1.1 Table   4.2

For thickness range is qualified for 25 mm ( 3mm to 2T) if i am correct.


2)   Regarding Position – PQR is qualified with 2G( Horizontal)

But in WPS welding Progression – Uphill. whether 2G can weld Uphill position. 


Please clarify me regarding above points.


Thanks and Regards

Kiran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eed99218-5c5c-42df-a5f2-dd072a39d346%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29Oja4tvx8VaJz5EeSaqZWWsJ7ZiR9G%3DGEYPbCCWpryCVFA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/16de0099-8223-4541-b773-69bf8c78cdc3%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


--

KIRAN

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMFjUk6Jd0JLRZYOZQqpmNci2jUhtRoyaPxsRw6V1ajmPGybsQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...