RE: [MW:29732] Difference in ASTM and ASME material

For additional explanation and examples of acceptable material see ASME Section II, Part A, Mandatory Appendix II, Basis for Use of Acceptable ASME, ASTM, and Non-ASTM Editions.  The examples delineated in II-200 (d) may be of some help.  Note that Table II-200-1 lists the construction code acceptability and editions (year) of ASTM specifications that are acceptable.

 

Also note, SA- and SB-, materials are those for which ASME Section II, Part D, code allowable stresses have been determined. 

 

Enjoy.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PGoswami
Sent: Tuesday, June 18, 2019 9:53 PM
To: materials-welding@googlegroups.com
Subject: RE: [MW:29729] Difference in ASTM and ASME material

 

ASTM is the originator of materials specifications . ASME adopted the ASTM grades for Boiler and Pressure Vessel Industries. In the process of acceptance and adoption some material were accepted as is , some were modified to suit design and application requirements in BPV environments.

Each ASME specification at the very beginning tells what're the differences between this ASME Grade vs the original ASTM grade.

On receipt of materials one should try to match the MTC to the PO requirements and the technical specifications, as sampled below. If the P.O indicates ASME but the vendor supplies ASTM grade, then at least a "Certificate of Conformance"  should be expected at the point of acceptance.

Thanks.

 

P.Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ramin Kondori
Sent: June 18, 2019 9:07 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:29724] Difference in ASTM and ASME material

 

Not all ASTM materials are qualified as per ASME standards.

Each ASME standard accepts ASTM materials based on the application.

 

Regards

Ramin  Kondori

Sr. QA/QC & Welding Engineer

-----------------------------------------------------------

PG-Dip. in Welding Engineering (IWE  AT  0070)

BSc. in Civil Engineering (IUT)

BGAS Painting Inspector

ASNT Level I&II

                        

IIW-Logo-Colour-small

 

 

On Fri, Jun 14, 2019 at 8:28 PM Pankaj Kolhe <pankaj.kolhe15@gmail.com> wrote:

Dear experts,

 

what is the difference in ASTM and ASME material. what care should be taken while reviewing MTC, and lab testing.

when can we say this material is acceptable as per ASTM OR ASME?

 

Pankaj

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA_HBVuSzAyetS1DzmjbzbP8%2BDN6L3PPx2ZCjDfuni9rbyJW6w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEagfUiHYzBAKFOV2ZDaPrXn97SBaRiLEzzu8qYFaJ-WbCsB4Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAAXTgG5ol1NBsdxd/DE0A8HCgAAAEAAAALDUdOtN%2BMBPiQ3PzXeAEfwBAAAAAA%3D%3D%40quickclic.net.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...