Thursday, May 23, 2019

Re: [MW:29631] I need to do dissimilar weld joint (6xxx series Aluminium to Steel). What filler wire should I choose?

You cannot weld aluminum to steel by arc welding..


Regards

Prem Nautiyal


PREM S NAUTIYAL
CELL : 9769316004





From: Ram <rameshsmit@gmail.com>
Sent: Thu, 23 May 2019 17:14:42 GMT+0530
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:29628] I need to do dissimilar weld joint (6xxx series Aluminium to Steel). What filler wire should I choose?

I need to do dissimilar weld joint (6xxx series Aluminium to Steel). What filler wire should I choose?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https:roups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7206cf51-d3f4-413a-838e-3036e9ad1a26@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1558611882.S.7494.3239.f4-234-218.1558622259.8889%40webmail.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...