Re: [MW:29628] As per Sec IX Welder Qualification Range for P43 to P43 GTAW

FM check QW 356 of 404.14 for and QW-416.
FNO check QW 404.15
SFA no XX, 

What do you mean by XX?? just keep as it is, change SFA will change process irrelevant of equivalent.

Regards
Muneeb


On Wed, May 22, 2019, 7:30 PM K K <karan.hbl@gmail.com wrote:
Dear experts,

Please let me know welder qualification range.

Details as below :

Actual Values

Pipe- Groove

1) P 43  To P 43 (SB-444)
2) GTAW ( Manual )
3) Thickness -5.54mm
4) SFA-5.14
5) F No- 43
6) Filler metal -ERNiCrMo-3
7) Position -6G

If I am not Wrong please check below i have mentioned Range Qualified.

Groove and Fillet Weld

1) P No - 1 thru 15F,34,41 thru 49
2) GTAW ( Manual )
3) SFA No- 5.xx
4) Thickness - 11.08mm
5) F no- 34,41,46
6) Filler metal - Any
7) Position - All

Please give me your feed back.

Regards
Kiran
 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a0641006-7a9d-438d-8a30-75a59731576f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANtRWKuhDtK0K30m4LJRMuUTEsTcJiPM4Gr2qgBW65AwEPZHxg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...