E-6013 is enough
On Fri, May 17, 2019 at 2:48 PM vaishakh <vaishakhmgr@gmail.com> wrote:
--I need solution for two issues1.We are using IS 2062 E-410 Grade material , for that E-7018 electrode is enough?2.For welding chequered plate can we select E-6010 over e-6013?
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/270eeebf-9744-406d-9e72-4f73d0b4f242%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8mTnz0JSfpyJOH0HB0jEExdf0m%3DE3A9ccrsx%3DgwtSGOCg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments