Wednesday, May 22, 2019

Re: [MW:29623] Electrode selection

You can use E-7018, E-6010 & E-6013 according to service requirement

On Wed, May 22, 2019 at 2:40 PM Vinay Thattey <vinay.thattey@gmail.com> wrote:
Should be OK

On Tue, 21 May 2019 at 15:04, vaishakh <vaishakhmgr@gmail.com> wrote:
Dear Experts,
 
         Currently we are using E-7018 electrode to weld IS 2062 E-410BR grade material.Please tell me wheather this electrode is enough to weld this grade material or should i go for E-8018. Please help me to solve this.
Thanks and Regards
Vaishakh.k.c.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/01e6f607-15c0-4a1f-a4e4-a0f45c85f872%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29OjNKBi%2B%2BnhabS2caCh_T4FJnQ6qvqQhioMJPSnonS-iNQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8n0h7kNzYJh7UZ02y56w0fFcMWn832FYccuFSpwO9L5Tw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...