235JR is P-No 1 because it is  listed in QW/QB-422 and not because of the chemical composition


Στις Τρί, 21 Μαΐ 2019 στις 12:34 μ.μ., ο/η 'MAGHROUD Moussa' via Materials & Welding <materials-welding@googlegroups.com> έγραψε:
1. PSWP as per ISO 15614
2. For S235 JR is CS, P N1, check chimic and mecanic analysis.  


Envoyé depuis mon smartphone Samsung Galaxy.

-------- Message d'origine --------
Date : 15/05/2019 12:54 (GMT+01:00)
À : Materials & Welding <materials-welding@googlegroups.com>
Objet : [MW:29588] Query for Code and S 235JR

Dear All,

Please clarify as per which code we can make the PWPS for SS water bar.

And Unlisted material like EN10025- 2 S 235 JR- how i can get the P.No. and which electrode shall i use for SMAW process.

Regards
K K

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/33988233-1a3a-4eb9-a0e5-a0e8c782a372%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5ce2b302.1c69fb81.84d3f.58f4SMTPIN_ADDED_MISSING%40gmr-mx.google.com.
For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40CgJJ%3D62SmcevJ3q0te%3DDCtoXCiC%3D3BsAvqpCkjiiTWiQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...