Saturday, May 18, 2019

Re: [MW:29598] Simulation heat treatment

Heat treatment is governed by Construction Code. 

Regards,
Prashant

On Fri, May 17, 2019, 2:48 PM chiluka venkatramulu <ramuluchiluka@gmail.com> wrote:
Dear All,
Pl clarify when we need simulated heat treatment for WPS as per ASME Sec-IX.

Thanks & Regards,
Venkatramulu

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF98%2BdF9791jG0wTQ%3DmPU5oU1B1QW%2BPVY4Pw2tufxCBF4YSBNg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAkMc%3D7MtkfEmGHJMaLNoyrdO9Rxs3Z1Mh7ywJmipudc8BGXdg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...