AWS A5.9 ER2594 shall be used.
Thanks,
Ruban Stanley S
On Fri, May 10, 2019 at 11:36 AM Ram <rameshsmit@gmail.com> wrote:
I need to weld Super Duplex Stainless Steel using MIG welding process. What filler wire should I choose it? Can someone recommend the filler wire for this?--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/03c718dc-0b11-457d-ab26-e1da274be17f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMPURfsAh5HuXixWLBNMsLuoy1Mgs2LYdiwQ1ZNCq_wZkn96zw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments