Re: [MW:29568] Electrode for Material SA516 Gr70

With E6013 you will not get strength you should go for E7018 electrode with low hydrogen content

Regards,

Rohan soni
8238850741

On 07-May-2019, at 6:41 PM, 'anand gupta' via Materials & Welding <materials-welding@googlegroups.com> wrote:

I think for SA 516 GR 70 is best electrode is E7018. 

Regards 
A p gupta 


On Tue, 7 May 2019 at 17:39, Kiran
Dear All,

Please refer below mentioned details and please let me know, can I use this details in PWPS as per D1.1.
 
1) Material -SA 516 Gr.70 to SA 516 Gr.70

2) P No- 1 Group No - 2 to P No- 1 Group No - 2

3) F No- 4
 
4) A No-1

5) SFA No- 5.1

6) AWS No(Class) -E-6013.

I have debut about electrode.  

If any thing please wright briefly.


Thanks and Regards

Kiran 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a45e40b7-5849-44b8-80b2-9c2551ce957c%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/828500067.1434857.1557234718674%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...