Dear Group
Just to share with you this indication.
It´s about a failure in the bottom zone of pressure vessel separator.
This is a thickness lost due to corrosion by bacteria or MIC as is mentioned in API 571
This indication has more than 2 meter in longitude and 0.6 meter in wide.
Nominal wall thickness 3/8".
Failure presented after 15 years in service of pressure vessel.
Regards
Miroslav Tadic
Integrity Engineer
API 581 IPC # 60883
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/B1C5C970BEA29243935FA5EB72F113C80362EFAB0D%40BOLEXVSG11.chaco.com.bo.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment