Yes, that the correct choice with respect to welding consumable. However it's a bad design with respect to materials selection if the Duplex Stainless Steel is the major pressure boundary materials and a part of the process stream.

API steels may be welded to DSS as support , under proper cathodic protection environments, not as direct Butt-Joints with the same process parameter envelopes.

 

Thanks.

 

P.Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of merghni
Sent: May 18, 2019 9:44 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:29598] WPS

 

 

Dear Colleague;

 

 

I have a question ,please i want to know how to select the filler metal to weld dissimilar metal ,because i have WPS , the information :  P1 to P10H ,Grade API 5L,PSL 2  , X65Q to Grade ASME A790 S31803 and  i found the electrode ER2209 for root and E2209-16 for fill is this selection acceptable or not i need advice  .

I review ASME IX but i didn't find any information about this.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/70916cb3-d5d3-4952-8d0c-aebe10c76f40%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...