Please see the extract  from ASME Sec-II, Pt-D, on the recommended temperature of applications for ASME designed components/systems . You should  read the  code so as to find additional information, including allowable stresses.

 

Thanks.

 

P.Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of krishna kamal nayan Pandey
Sent: April 30, 2019 7:25 AM
To: materials-welding@googlegroups.com
Subject: [MW:29539] A 234WPB

 

Gents,

Can anyone confirm the temperature range of A 234 WPB fittings. 

I mean the temperature this grade fitting can resist?

 

Best Regards,

 

Krishna Kamal Nayan  

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...