[MW:28836] Re: Use of ss309 electrode in cracked area

pl provide details it is pipe or plate and whats thickness?

On Friday, December 28, 2018 at 3:13:39 PM UTC+3, Gopalakrishnan G wrote:
Dear experts
Whether it is advisable to use ss309 electrode to arrest the crack in mild steel material .As my job is fully machined it is difficult to completely remove the crack.kindly guide me.

--