Re: [MW:28564] Combined PQR

Hi,

my interpretation of the clause 3.6.1 is as follows;
A combination of, QUALIFIED and PREQUALIFIED WPS'S   = I interpret this as either qualified WPS+qualified WPS, Qualified+Prequalified or Prequalified+Prequalified. 
..may be used without any requalification for the combination.

So it nowhere states that existing qualified combinations can be split into 2 separate WPS's.

Above is my interpretation, 

On Fri, Nov 2, 2018 at 10:41 AM Ramesh <rameshkannandevaraj@gmail.com> wrote:
Hi Nithin,

i am unable to find the word " independent PQR's may be combined " in above clause

i presume, this clause does not say about PQRs, Only your final WPS ( which may have single supporting PQRs or process or combined PQRs or process) 

These qualified WPSs can be combined  without combination and within limitations of each process ( refer last two para carefully ) 

i understand from response that, suppose if an PQR have with combination process ( Ex.TIG+SMAW)  , u are interpreting that preparing Two separate WPS ( one for TIG & one for SMAW)  is not allowed as per D1.1. right ? 

or, Pl explain your interpretation of above 3.6.1 clause.  


Thanks and Regards


Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



On Fri, Nov 2, 2018 at 10:30 AM Nithin Joseph <nithindsilva4u@gmail.com> wrote:
Dear Mr. Rameshkanna,

Note that clause 3.6.1 clearly states independent PQR's may be combined and does not state WPS's can be made from the combination PQR.

On Thu, Nov 1, 2018 at 7:54 AM Ramesh <rameshkannandevaraj@gmail.com> wrote:

Hi 

shakin thobias

 

1. Please refer AWS D1.1 , Part C for performance qualification requirements.

Range of qualifications - pl refer Table 4.10 & 4.11

 

2. Combination of WPS is allowed as per 3.6.1  This is applicable for both qualified or prequalified WPS.[ Screen shot from 2015 edition as below ]




Also refer OLD AWS interpretation as below [ 1984 edition]






Thanks and Regards


Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



On Wed, Oct 31, 2018 at 10:06 AM Nithin Joseph <nithindsilva4u@gmail.com> wrote:
In AWS there is no provision of extracting a process. for eg, you are qualifying FCAW+SMAW, you have to use same combination on job too. Writing separate WPS for SMAW & FCAW is not acceptable as per AWSD1.1.

On Wed, Oct 24, 2018 at 2:11 PM shakin thobias <shakinthobias@gmail.com> wrote:
Dear experts

I need to qualify welders in Both FCAW and SMAW. can i do both qualification in same PQR. what are the parameters and range of qualification. qualify that welders to max 30 mm thickness range. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Regards,
Nithin Joseph Dsilva
+971 557645785

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Regards,
Nithin Joseph Dsilva
+971 557645785

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Regards,
Nithin Joseph Dsilva
+971 557645785

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...