Hi Nithin,

i am unable to find the word " independent PQR's may be combined " in above clause

i presume, this clause does not say about PQRs, Only your final WPS ( which may have single supporting PQRs or process or combined PQRs or process) 

These qualified WPSs can be combined  without combination and within limitations of each process ( refer last two para carefully ) 

i understand from response that, suppose if an PQR have with combination process ( Ex.TIG+SMAW)  , u are interpreting that preparing Two separate WPS ( one for TIG & one for SMAW)  is not allowed as per D1.1. right ? 

or, Pl explain your interpretation of above 3.6.1 clause.  


Thanks and Regards


Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



On Fri, Nov 2, 2018 at 10:30 AM Nithin Joseph <nithindsilva4u@gmail.com> wrote:
Dear Mr. Rameshkanna,

Note that clause 3.6.1 clearly states independent PQR's may be combined and does not state WPS's can be made from the combination PQR.

On Thu, Nov 1, 2018 at 7:54 AM Ramesh <rameshkannandevaraj@gmail.com> wrote:

Hi 

shakin thobias

 

1. Please refer AWS D1.1 , Part C for performance qualification requirements.

Range of qualifications - pl refer Table 4.10 & 4.11

 

2. Combination of WPS is allowed as per 3.6.1  This is applicable for both qualified or prequalified WPS.[ Screen shot from 2015 edition as below ]




Also refer OLD AWS interpretation as below [ 1984 edition]






Thanks and Regards


Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



On Wed, Oct 31, 2018 at 10:06 AM Nithin Joseph <nithindsilva4u@gmail.com> wrote:
In AWS there is no provision of extracting a process. for eg, you are qualifying FCAW+SMAW, you have to use same combination on job too. Writing separate WPS for SMAW & FCAW is not acceptable as per AWSD1.1.

On Wed, Oct 24, 2018 at 2:11 PM shakin thobias <shakinthobias@gmail.com> wrote:
Dear experts

I need to qualify welders in Both FCAW and SMAW. can i do both qualification in same PQR. what are the parameters and range of qualification. qualify that welders to max 30 mm thickness range. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Regards,
Nithin Joseph Dsilva
+971 557645785

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Regards,
Nithin Joseph Dsilva
+971 557645785

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...