Dear muneeb sir,
Where you get max hardness value 250 hen please say paragraph details .
Need for reference
Regards
Sangram
Sent from my iPhone
check 331.1.4 of ASME B31.3The Maximum allowable hardness is VHN 250HVRegards,M.Muneeb
--Date: 2018-10-30 15:44Subject: [MW:28529] SA335 Gr.P91(P-15E)Dear experts ,If some one have working experience with p91 material; please help regarding heating & cooling rate. Max hardness allows .My construction code is Asme B31.3Please specify the code details.Sent from my iPhone-----You received this message because you are subscribed to the Google Groups "Materials & Welding" group.To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.Visit this group at https://groups.google.com/group/materials-welding.For more options, visit https://groups.google.com/d/optout.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments