Monday, May 7, 2018

Re: [MW:27789] RE: 27787] Welding oF dissimilar metal at High temperature(Micro Alloy+P11)

Dear Sir,

The tubes are centrifugally cast and chemical composition  is  below.

Grade G 4852 Micro(25Cr 35Ni Nb)
 
C 0.45,Si 0.7,Mn 1.5
Cr25, Ni 35,Nb1
P 0.03,S0.03,W0.6,Ti,0.3,
Pb 0.01,Sn,0.01,Zn,0.01


Regards,

Asif Shahzad


On ‎Sunday‎, ‎May‎ ‎06‎, ‎2018‎ ‎06‎:‎38‎:‎15‎ ‎PM, PGoswami <pgoswami@quickclic.net> wrote:


What's the micro alloy to be welded? What' the manufacturing condition. Could you attach the MTR or any other appropriate details?

 

Thanks.

 

 

P.Goswami.P.Eng, IWE.

Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

 

From: 'Asif Shahzad' via Materials & Welding [mailto:materials-welding@googlegroups.com]
Sent: May 6, 2018 4:41 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:27787] Welding oF dissimilar metal at High temperature(Micro Alloy+P11)

 

Dear Expert,

 

We want to weld Micro alloy (Ni,Cr) furnce tubes with the P11reducer in the Steam methane reformer that will be operator at 850 to 900 C temperature.

Please provide your opinion about welding reliability of these two dissimilar   metal at high teperature.

 

Regards,

Asif Shahzad 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...