Re: [MW:27782] Change in WPS & PQR

Yes, you can update for this code revision clearly stated in revision..it is allowed

On Fri 4 May, 2018, 2:23 PM Manivannan Hemu, <hemumanivannan@gmail.com> wrote:
Hi,

You may refer to QW 200.2[c].

Regards,
MANIVANNAN.P

On Fri, May 4, 2018 at 1:44 PM, S. Kharwar <sanjay.singh349@gmail.com> wrote:
Dear Experts,

Can anyone suggest..

I have an Old WPS in ASME Sec.IX  with Material Grade IS 2062  E250 B  in   unassigned  material number  , now I would like to use  but the inspector said that currently  it is in Assigned -P1  number .
So can I change my WPS  front page with revision by editing as Assigned number , similarly in PQR .

Is it mentioned any where in ASME Sec.IX .


Thankyou

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...