Re: [MW:26843] SR equirement for Heads

Nothing is mentioned in GA.
Buy EIL spec says SR is reqd. For below 16 mm and NR for above 16mm.
As per code checked but fibre el. Is below 5%


On 28 Sep 2017 07:47, "PREM SHANKARDUTT NAUTIYAL" <prem_nautiyal@rediffmail.com> wrote:
Follow the heat treatment data written in your approved GA drawings.

PREM S NAUTIYAL

CELL : 9769316004


From: Pankaj Kolhe <pankaj.kolhe15@gmail.com>
Sent: Tue, 26 Sep 2017 21:19:03
To: materials-welding <materials-welding@googlegroups.com>
Subject: [MW:26837] SR equirement for Heads
 
Dear Experts,
 
AS per IL spec.all cold formed heads need to be stress relieved.
we have 6mm,10mm,12mm,16mm & 20 mm thk dish end in our job.
 
so my question is shall i do SR for all thickness dish end or how to proceed.
 
MOC 516-70

 
pankaj

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...