Wednesday, September 27, 2017

Re: [MW:26838] SR equirement for Heads

Follow the heat treatment data written in your approved GA drawings.

PREM S NAUTIYAL

CELL : 9769316004


From: Pankaj Kolhe <pankaj.kolhe15@gmail.com>
Sent: Tue, 26 Sep 2017 21:19:03
To: materials-welding <materials-welding@googlegroups.com>
Subject: [MW:26837] SR equirement for Heads
 
Dear Experts,
 
AS per IL spec.all cold formed heads need to be stress relieved.
we have 6mm,10mm,12mm,16mm & 20 mm thk dish end in our job.
 
so my question is shall i do SR for all thickness dish end or how to proceed.
 
MOC 516-70

 
pankaj

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...