Wednesday, September 27, 2017

Re: [MW:26838] Impact test requirement for JO and JR grades in structural fabrication.

in which specification it is mention about thickness > 6mm , 

On Saturday, 10 September 2011 19:15:33 UTC+4, Harish wrote:
Impact test is mandatory for t>6mm, if the material is going for low temperature service.

2011/9/10 arvinda shan <arvin...@gmail.com>
Dear Experts,
 
For crosshead installation in jetty project, the following materials (37mm) are used.
 

Road way            - S355JO

Crosshead           - S355JR & S275JR

Pipe track            - S355JR

 

As per European structural steel standard EN10025 , for JR grade, Longitudinal charpy V-notch impacts 27J @20 degrees and for JO grade, Longitudinal charpy V-notch impacts 27J @ 0 degrees.

 

We received materials mill certificates w/o impact test.

 

My question is whether impact is mandatory for above grades or any criteria of thickness as per EN10025? Please mention with reference codes.

 

Your valuable suggestions are appreciated.

 

Regards

 

arvinda

 

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
regards,
Harish.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...