Wednesday, September 13, 2017

Re: [MW:26819] Acceptance Criteria

For Steel structural items you can propose NDT as per AWS D1.1. Acceptance criterias are given for all NDT.

On Fri, Sep 8, 2017 at 7:56 AM, Vijay Joshi <hivijay1970@gmail.com> wrote:
Friends,
Many time for some odd jobs, we find the contractor is not clear on what is acceptable when NDT is conducted.
For example, we had to UT some welds on a repaired columns of a gantry crane.
There was no reference Code of construction.
Therefore, will you please help me in knowing what Codes are applicable to what type of jobs and what is their respective acc criteria references?
Thanks,
Vijay

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...