Hi Vijay,

What is the piping class and MDMT of this pipe, you may refer in your Client approved PMS .

Get the temperature from PMS, then you will come to know the impact testing requirement and temperature.

With kind regards
P Govindan

On Sep 7, 2017 13:30, "savadqac@gmail.com" <savadqac@gmail.com> wrote:
Hi,

As per project spec or if specified minimum @ -29, only if C/Mn less than 5
Savad

Sent from my Huawei Mobile


-------- Original Message --------
Subject: [MW:26794] ASTM A106 grade B pipe
From: vijay panchal
To: Materials & Welding
CC:


is impact test required for ASTM A106 grade B pipes??? and is yes what will be the testing temperature?

Vijay

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...