Thursday, September 7, 2017

Re: [MW:26797] ASTM A106 grade B pipe

Not required, if it has to be done it will be on the MDMT, 

Regards,
Anthony.

On Thu, Sep 7, 2017 at 10:23 AM, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (materials-welding@googlegroups.com) Add cleanup rule | More info

What is the Design Code & Minimum Design Metal Temperature(MDMT).
 
Thanks & Regards
J.Gerald Jayakumar
0091-9344954677



From: vijay panchal <vijayvp89@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Thursday, September 7, 2017 8:51 AM
Subject: [MW:26794] ASTM A106 grade B pipe

is impact test required for ASTM A106 grade B pipes??? and is yes what will be the testing temperature?

Vijay
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...