Re: [MW:26795] ASTM A106 grade B pipe

It's not required as they are designed for moderate and high temperature service. But if project specifications as for, it will be MDMT or service temperature.

Thanks & Regards,
Harish

On Sep 7, 2017 8:51 AM, "vijay panchal" <vijayvp89@gmail.com> wrote:
is impact test required for ASTM A106 grade B pipes??? and is yes what will be the testing temperature?

Vijay

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...