Re: [MW:26793] IS IGC test Required ?

Akash,
For the intended service IGC test is not required unless asked for by client. If water contains diluent of acids or may be required subject to client's discretion. 
Thanks 
P Goswami, P.Eng , IWE.




Sent from my Bell Samsung device over Canada's largest network.

-------- Original message --------
From: 'james gerald' via Materials & Welding <materials-welding@googlegroups.com>
Date: 2017-09-06 03:29 (GMT-05:00)
To: materials-welding@googlegroups.com
Subject: Re: [MW:26792] IS IGC test Required ?

Any welding involved.
 
Thanks & Regards
J.Gerald Jayakumar
0091-9344954677



From: Aakash <harenathjha@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Wednesday, September 6, 2017 10:03 AM
Subject: [MW:26790] IS IGC test Required ?

Hello Expert,
Following are the situation,
Material, SA 312 Typ 304 L (Carbon content is >= 0.03 %)
Joining process :- Welding by GTAW process
Service Temprature -90 Degree (MAximum)
Pressure - 7kg/cm2 (maximum)

Service fluid :- Water,

Is IGC Test ( ASTM 262) is required to be carried out ?

As per my understanding, it is not required.

You please give your advice

Regards
HNJ
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...