this requirement governing from Project specification & standards.

thanks.
Ahmed 

On Wed, Sep 6, 2017 at 9:47 AM, Aakash <harenathjha@gmail.com> wrote:
Hello Expert,
Following are the situation,
Material, SA 312 Typ 304 L (Carbon content is >= 0.03 %)
Joining process :- Welding by GTAW process
Service Temprature -90 Degree (MAximum)
Pressure - 7kg/cm2 (maximum)

Service fluid :- Water,

Is IGC Test ( ASTM 262) is required to be carried out ?

As per my understanding, it is not required.

You please give your advice

Regards
HNJ

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...