[MW:26830] QW 200.4

Gents,

I have two PQRs for 10mm and 38mm of GTAW+FCAW process.

I believe, i can prepare the WPS using the above PQRs for FCAW for Single V (w/ backing strip) and Double V (with back gouging) for the max thickness range of 1.5 to 200mm. 

Please share your information.

--