Dear Mr Kumar,

We are also facing the same issue, kindly share your corrective action was taken for close out.

Awaiting your valuable response.

With Kind Regards

P Govindan 
+965-60727159

On Tue, Dec 10, 2013 at 12:57 PM, Kumar <sk7920541@gmail.com> wrote:

Dear team,
Even as per A6  the issue doesnt solve..here the distortion is not localised or in spots as iterated in 650..the whole shell id has come inside for around 12.5mm as mean and 1.5 mtr around 19-20mm in particular...so my queries are;
1. Is 650 calling for any welding distortion allowence?
2.is there any fillet sizing given for stiffeners particularly?
3. Could we club aws d 1.1 by any means to 650?
Now the sub-contractor is challenging us for back-ups in terms of rejection and rectifications
Anyhow the radius limitation is 19mm...which has been crossed in that area at least.. help with your valuable responses pls.
Thanks in advance,
Kumar

On Dec 9, 2013 4:16 PM, "Jorge Mejía Lema" <jmejialema@gmail.com> wrote:
Please, see  ASTM A6 referred for API 650.
Regards,
jml


2013/12/7 Kumar <sk7920541@gmail.com>

For a tank shell course thickness 8mm, intermediate stiffner welding done below the wind girder to fillet size 8mm...now the plate has buckled towards throughout ID for almost 10 to 14 mm...this is the last shell course(tank height 20, od - 36 mtr)..how can decide this buckling is within tolerence?....pls. share your opinions..
Thanking in advance
Kumar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...