Tuesday, November 1, 2016

Re: [MW:25642] Damaged RF

You can refer ASME PCC1 or PCC2 according to your requirements . Gives you the acceptance criteria and machining allowances .


On 1 Nov 2016 3:23 p.m., "baskaran subramaniyan" <baskaran.avc@gmail.com> wrote:
Hai,

See ASME B16.5 Cluase 6.4.6 for acceptance on Flange Facing Finish Imperfections.

Verify with the comparator for machining finish

Generally 3.2 to 6.4 micrometers AARH is acceptable.

On Mon, Oct 31, 2016 at 4:46 PM, sam m <samuvel.masilamani@gmail.com> wrote:
Confirmation for the flange face roughness (AARH) -usually reported in microns inch against the standard requirements (e.g ASME B16.5)shall be produced as an evident 

Regards 
Sam


On Monday, 31 October 2016, Vijay Joshi <hivijay1970@gmail.com> wrote:
Dear experts,
A  2" RF WN flange gasket (or raised surface) area got blasted by oversight and NCR was raised by our client. We have done milling -machining on the surface to restore the raised face and it looks OK and acceptable but the client is asking for machining report.
How is it done, I mean to confirm that the flange is acceptable?
Can we see a standard report of such machining.

Thankfully,
Vijay Joshi

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABbs01aj%3D8jD6CzSWL4KOPu76BSg__RvWCBfzc2D%2B0reKr_wRA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


--
Sent from Gmail Mobile

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFTCtEA2mf6h7w%3DAekcoB%2BP7r2Yv8c2W8_zLS%2BspBW5rABHKpA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Regards

Baskaran Subramaniyan
+919884434742

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADFcTk%3DRdK-tRR1qsyx5E3coLt0aanwOB-Lbm_DkJ5bhVKKjBQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKT-TuoxQjemxXWs3jx0dGe_%2BCwg-hna-5PpvHEHOPyH0rQq5A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35763] Hardness range for CS+ Alloy0625 clad welding