Dear Expert,

As precautionary measure we have selected Hyper Duplex 2707 as welding material for the reactor. In principle 2707 HD is considered as a grade higher than 2507 as far as PREN is concerned, owing to which we brought it into the picture.

We wish to know your feedback on the quality of welding attained with this combination and corrosion resistance of weld joints as it goes through heat transition during welding.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/dcd81c99-fda1-4e34-a1bf-7445638d6707%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...