RE: [MW:25509] Usage of ASME Sec 9 WPS for sub contractor

John Henning is absolutely correct. All the more flexible answers given previously are incorrect if you need to be code compliant.

 

Alan Denney

AKD Materials Consulting Ltd

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of John Henning
Sent: 07 October 2016 18:16
To: materials-welding@googlegroups.com
Subject: RE: [MW:25508] Usage of ASME Sec 9 WPS for sub contractor

 

Sorry guys – incorrect answer. 

 

For ASME B&PV fabrication, WPS's and PQR's may not be transferred, given, swapped, or sold between independent companies.  The only situation where another company or subcontractor can use your WPS's if the other company or subcontractor works solely under the control of your QC program (such as might happen if you hired temporary welders) .  You also need a provision in your quality control program documentation to describe how this is going to implemented.

 

Too many incorrect answers to this one.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of syed moinul hasan
Sent: Thursday, October 06, 2016 10:18 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:25497] Usage of ASME Sec 9 WPS for sub contractor

 

No issue indeed, as long as there is a mutual consensus by both party.

Cheers

Syed Moinul Hasan

 

On 6 October 2016 at 22:00, 'anand gupta' via Materials & Welding <materials-welding@googlegroups.com> wrote:

Dear 

as per ASME SEC IX you can not use wps of another party.

But another part have give written permission to use wps and your client accepted then you can use the wps.

 

Regards

a p gupta

 

On Tue, 4 Oct, 2016 at 18:16, thulaib arakkal

Dear All,

 

We have sub contracted our pipe welding work based on ASME B31.3 and ASME sec IX qualified WPS to another organization. Is it allowed in ASME section IX for a sub contractor to use the main contractor's WPS.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL2L2JMBzSCg4sYKoc2SsFKSEMEQRi-YwMBpOpAnY%3DQM-gH-JQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/498559274.9392695.1475776831560%40mail.yahoo.com.


For more options, visit https://groups.google.com/d/optout.

 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMXKe_ov-fjWLptrMfprLgj4Voa0WJovB3F6eTuYdNgrjnE3rA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/MWHPR03MB281619451AEBB4A12255DF86A1C60%40MWHPR03MB2816.namprd03.prod.outlook.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...