[MW:25487] Re: GMAW for CS

Try again with new batch filler

On Tuesday, October 4, 2016 at 2:09:12 PM UTC+5:30, MAGHROUD Moussa wrote:


Dear experts

I am trying to qualify a PQR using GMAW applied on a plate spec A36,10 mm thick, ER 70S6 1.2 mm, position 3G, progression downhill and Argon pure as shielding gas. But after RT shooting we find porosity throughout the joint. 
Please anyone can help how to qualify this weld. 


Envoyé depuis un mobile Samsung

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/becfa1bc-61fa-4b3e-80b4-3d65b5c076c9%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...