Wednesday, October 5, 2016

[MW:25486] Requirement For Shoe Support Pad

Gentlemen s ,

I have 2" to 10" P1 material pipe for Thermic Fluid of design temperature is 250 degree cel. Drawing shows trunnion and shoe supports directly fully welded on the pipes of thickness range 2 to 10 mm . Pls suggest whether its acceptable or need to have a reinforcing pads which is not welded to pipe will be acceptable. 



Thanks in advance

Pratish

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f8ebb28b-de9b-4bd2-b909-adecf8cdd972%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...