Saturday, August 6, 2016

Re: [MW:25207] RE: 25195] PQR Qualification.

F&A nos not essential for welding operators


On 06-Aug-2016 9:57 am, "Lakshman Kumar. B" <lakshmankumar4@gmail.com> wrote:

Hi,

It will not qualify…

As F no & A No are not only the criteria for acceptance…

F&A grouping are majorly for welder / operator qualification and not to consider in PQR.

Need to go for a fresh PQR.

 

Thanks & Regards,

Lakshman Kumar B,

+91 9440031459.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of r.vroom
Sent: Friday, August 05, 2016 8:01 PM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:25195] PQR Qualification.

 

All,

 

Please advice me in the following.

ASME IX :2013

Weld coupon base material P8 (ASTM A240 TP 316) to P1 (S333 Gr. 6)

FCAW: Filler metal Bohler CN 23/12 Mo PW-FD (E309LMoT1-4)

 

Does this PQR qualify a weld joint P8 (ASTM A240 TP 304) to P8 (ASTM A240 TP 304)

by changing filler metal into E308LT1-1 for both F No. 6 and A No. 8

 

Follow Table QW 255 Ø P-number qualified article 403.11 -> article 424.1 I should say no, but am I right ????

 

 

Diameter and thickness are in range.

 

Thank you.

 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/83ce3674-8b7a-42d2-b8f6-98aa0cdb35db%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/008701d1ef9a%2486d40920%24947c1b60%24%40gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOF7OM237Ok%2B7xpTW196AJOnAE%2Be5aD2XG3tM0ZLdr5Yg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...