Saturday, August 6, 2016

Re: [MW:25201] Intermediate stress relief treatment

Preheat Maintenance is a Supplementary Essential Variable for Procedure Qualification. I.e applicable when impact test is required by the Design Code. So if Engineering (ARAMCO) rerquires post heating, you have to make a PQR with post heat maintenance

2016-04-07 8:29 GMT+03:00 'Neilashkumar' via Materials & Welding <materials-welding@googlegroups.com>:


Dear All, 

Good Day ! As per our client aramco , insisting us to do dehydrogenation treatment for P11 material after welding completion for four hours prior to PWHT.

Please clarify whether post heat maintainence for 4hours is mandatory for fillet weld.

As per our WPS  I am doing it for  groove joints , it is clad vessel for 145 inch diameter ... 

Above that insulation and pad welding Accor , is there any clause given in ASME section states that post heat maintainence is not required for P11 material.


As per aramco standard SAESW014 General it is given


P.NEILASHKUMAR 
Sent from my iPad
MOB : 966 551094590
            + 91 9952110791

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0B59ABE0-AA41-4BD5-9389-F1AF70590CAB%40yahoo.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40C0jwBR75vgnAqj3dMLiLG5BSaUR%3DWpD4m1q3%3Drd5iMzA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...