Friday, August 5, 2016

Re: [MW:25195] A105 vs A216 Gr. WCB

Hi,

    A105 is forging material and A216 WCB is a casting material. I can suggest forging material is better than casting and also plug material will worn out during more operation. So you select A105.

Regards,

Karthikeyan


On 4 Aug 2016 12:45 pm, "Zihni Hakim" <muhammadzihnihakim@gmail.com> wrote:
Hello,
Is there anyone know the material differences from ASTM A105 and A216 Gr.WCB?
because, if i've seen it based on the chemical and mechanical properties, they're all the same..
Anyone can tell, when we should use A105 or A216?

Nb : It is to be used for Plug Valve Material in pipeline engineering
Any help would be apreciated,
Thankyou


Best regard,
Zihni

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6318ec8b-444b-4b70-aeec-8eedb4e6e4ab%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC43g4k0Xh2De4-f%2B4F5AbsCpdLhq_w-q%2B5mVLjb4yvU8AAeAw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...