Wednesday, August 3, 2016

[MW:25190] Use of Full penetration WPS for Partial penetration

Dear All,

I have a requirement of partial penetration for single bevel weld joint. Required weld deposit thickness is 10mm & base metal thickness is 40mm. & material is INC625 to CS.

 

I have Qualified WPS for dissimilar thickness which is qualified for 11 mm weld deposit thickness & 70 mm base metal thickness.

My Question is Can I use full penetration WPS for partial penetration joint. 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eaaa262b-eebd-4afd-9376-833729743a96%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...