Monday, August 1, 2016

[MW:25179] Pipeline hydro test sectioning.


Does any specific requirement for hydro test sectioning method?
If pipeline is going more than 100 KM how do we handle the hydro test?
I suppose it is not possible to test one time due to the cost and time.

My question is as below;
1. The permanent flanges are required for sectioning for test? Or normally it is done by temporary flange?
2. If we need permanent flanges for test, how can I choose the location of flange?


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1d0888f3-0736-4206-a148-b76447ca867b%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...